• <tr id='eKziM9'><strong id='eKziM9'></strong><small id='eKziM9'></small><button id='eKziM9'></button><li id='eKziM9'><noscript id='eKziM9'><big id='eKziM9'></big><dt id='eKziM9'></dt></noscript></li></tr><ol id='eKziM9'><option id='eKziM9'><table id='eKziM9'><blockquote id='eKziM9'><tbody id='eKziM9'></tbody></blockquote></table></option></ol><u id='eKziM9'></u><kbd id='eKziM9'><kbd id='eKziM9'></kbd></kbd>

    <code id='eKziM9'><strong id='eKziM9'></strong></code>

    <fieldset id='eKziM9'></fieldset>
          <span id='eKziM9'></span>

              <ins id='eKziM9'></ins>
              <acronym id='eKziM9'><em id='eKziM9'></em><td id='eKziM9'><div id='eKziM9'></div></td></acronym><address id='eKziM9'><big id='eKziM9'><big id='eKziM9'></big><legend id='eKziM9'></legend></big></address>

              <i id='eKziM9'><div id='eKziM9'><ins id='eKziM9'></ins></div></i>
              <i id='eKziM9'></i>
            1. <dl id='eKziM9'></dl>
              1. <blockquote id='eKziM9'><q id='eKziM9'><noscript id='eKziM9'></noscript><dt id='eKziM9'></dt></q></blockquote><noframes id='eKziM9'><i id='eKziM9'></i>

                关键词搜索:碰焊机储能点焊机螺母点焊机中频逆变点焊机

                当前位置首页 » 新闻资讯 » 常见问题 » 铝棒对焊机如何解决焊接面发黄?

                铝棒对焊机如何解决焊接面发黄?

                返回列表 来源:安嘉 浏览:- 发布日期:2021-08-16 15:15:10【

                现在使用铝棒对焊机不仅仅满足于焊接牢固,而是对于焊接效果的美观性有更高的要求,光滑且不发黄。为什么焊接后会发黄呢?有哪些解决方案呢?

                铝棒对焊机

                焊接表面发黄的原因,一般是焊接时间偏长,通过调试,加大焊接气压,减少焊接时间,加强电极的冷却,可以有效解决此类问题。

                操作铝棒对焊机时,上电极下压,在两金属中间,形成一定的电阻,而焊接的电流,从一方流向另一方的过程中瞬间进行电熔接,所以不会出现发黄的现象。

                苏州安嘉自动化设备有限公司是从事自动化装配、焊接、检测设备和生产流水线的研制企业,主要应用于家电五金、汽车制造、钣金、3C电子行业等。可根据客户需求,研发定制各种需求的焊机和自动化焊接设备及装配焊接生产线、流水线等,为企业转型升级提供合适的自动化整体解决方案,助力企业快速实现由传统生产方式向中高端生产方式转型升级的服务。如果您对我们的自动化设备和生产流水线感兴趣,请联系我们:400-8333-566。





                转载请注明出处:安嘉对焊机www.szagera.com(对焊机厂家